Böhler Welding · Low-hydrogen 1 % Ni electrode · E8018-C3
Equivalent at Ador Welding
Tenalloy 70C
Listed under the same AWS classification: a direct equivalent for the same job.
This reference lists no product from the brand in this class or its nearest classes.
Chosun Welding · KOBELCO Welding · Nippon Steel Welding · Oerlikon Welding
AWS A5.5 · Low-hydrogen potassium, iron powder electrode, 80 ksi (550 MPa), all positions, AC or DC+, 1 % Ni (Cr and Mo limited).
Equivalents come from the makers' catalogues and websites. Check your welding procedure before substituting.
Higher-strength structural, offshore and ship steels that need toughness at −40 °C.