- Heat source
- Arc between a non-consumable tungsten electrode and the workpiece
- Shielding
- Inert gas — argon, helium or Ar/He (ISO 14175 I1, I3); Ar/H2 for some austenitic stainless
- Filler / consumables
- Bare rods or cold/hot wire — AWS A5.18 (ER70S-2/-6), A5.28, A5.9, A5.10, A5.14, A5.16 — or none (autogenous)
- Power source
- Constant-current; DC electrode negative for steels, AC for aluminium and magnesium; HF or lift-arc start
- Materials
- Practically all weldable metals: steels, stainless, aluminium, magnesium, titanium, copper, nickel, zirconium
- Thickness
- About 0.3 mm upward; root passes on any thickness
- Positions
- All positions
- Deposition
- Low — roughly 0.5–1.5 kg/h (higher with hot-wire)
- Operation
- Manual, orbital, mechanized