Nippon Steel Welding · 低水素系 3½ % Ni 溶接棒 · E8018-C2
Equivalent at Ador Welding
Tenalloy 70B
同一の AWS 分類に掲載:直接の相当品
同系統で表示記号が異なる(例:被覆剤の末尾記号):注記をお読みください
このリファレンスには該当分類の製品が掲載されていません
Atlantic · Böhler Welding · Chosun Welding · Golden Bridge · Hobart Brothers · Hyundai Welding · KOBELCO Welding · Lincoln Electric · Oerlikon Welding · Welding Alloys
AWS A5.5 · Low-hydrogen potassium, iron powder electrode, 80 ksi (550 MPa), all positions, AC or DC+, 3.5 % Ni.
Equivalents come from the makers' catalogues and websites. Check your welding procedure before substituting.
3.5 % Ni steels (e.g. ASTM A203 Gr D/E) for low-temperature service to about −73 °C.