Welding AlloysWA SPEEDARC 7018-EE7018E7018-H4 (EN ISO 2560-A E 46 4 B 3 2 H5)
Classification properties
What the code means
ECovered electrode
7070 ksi (490 MPa) min. tensile
2Flat and horizontal fillet only
8Low-hydrogen potassium, iron powder, high recovery — AC or DC+
AWS A5.1 · Low-hydrogen potassium, iron powder, high recovery electrode, 70 ksi (490 MPa), flat and horizontal fillet only, AC or DC+; impact 27 J at −18 °C.
Standart
AWS A5.1
Equivalents come from the makers' catalogues and websites. Check your welding procedure before substituting.
SI / metrik
E4928
ISO karşılığı
ISO 2560-B: E4928
Örtü / tip
Low-hydrogen potassium, iron powder (high recovery)
Pozisyonlar
Yatay ve yatayda köşe kaynağı
Akım
AC veya DC+
Çekme dayanımı
70 ksi (490 MPa)
Akma dayanımı
58 ksi (400 MPa)
Uzama
22 %
Darbe tokluğu (CVN)
27 J at −18 °C
Typical use
High-recovery low-hydrogen electrode for heavy flat and horizontal fillets that need crack resistance.