Choose a country to see its standard's plate, sheet and coil grades β and the closest match in the other seven systems.
Standards Australia & Standards New Zealand Β· AS/NZS
β 250 MPa structural
Grade 250
Same class: ASTM A36 Β· EN S235JR/S275JR Β· IS E250 Β· GOST C245/C255 Β· GB/T Q235B Β· KS SS275 Β· JIS SS400
β 350 MPa structural
Grade 350
Same class: ASTM A572 Gr 50 Β· EN S355JR Β· IS E350 Β· GOST C345/09G2S Β· GB/T Q355B Β· KS SM355 Β· JIS SM490/SM490Y
Pressure vessel (β A516 Gr 70)
β
No direct equivalent listed. Elsewhere: ASTM A516 Gr 70 Β· EN P355GH Β· IS R260 Β· GB/T Q345R Β· JIS SGV480
| Standard | Grades |
|---|---|
| Mild structural | |
| AS/NZS 3678 | 250, 300 |
| High-strength / HSLA | |
| AS/NZS 3678 | 350, 400, 450, WR350WR350 β weathering |
| Pressure vessel & boiler | |
| AS 1548 | PT430, PT460, PT490 |
| Standard | Grades |
|---|---|
| Hot-rolled sheet & coil | |
| AS/NZS 1594 | HA1, HA3, HA250, HA300, HA350, HA400, HU300, HW350 |
| Cold-rolled sheet & coil | |
| AS/NZS 1595 | CA4, CA220, CA260CA series |
| Hot-dip coated (zinc / Al-Zn) | |
| AS 1397 | G2, G3, G250 β G550Z zinc / AZ Al-Zn |
Ship plate uses the same IACS grades in every system: A, B, D, E and AH / DH / EH / FH 32 Β· 36 Β· 40 β certified by ABS, LR, DNV, BV, CCS, KR, NK or RS.
| Application | Specify | Note |
|---|---|---|
| Structural plate | ASTM A36 / A572 Gr 50 β or EN S275JR / S355JR | Most Saudi project specifications call ASTM or EN |
| Pressure-vessel plate | ASTM A516 Gr 70 | EN alternative: P355GH |
| Equivalent stock (GB/T, JIS, KS, IS) | Offer only as an approved equivalent | Dual-certified mill test certificate required |
| Item | What to state | Example |
|---|---|---|
| Standard & edition | Full designation with year | EN 10025-2:2019 |
| Grade | Strength grade | S355 |
| Sub-grade | Impact class / test temperature | J2 (27 J at β20 Β°C) |
| Size | Thickness Γ width Γ length | 20 Γ 2000 Γ 6000 mm |
| Certificate | Inspection document β dual-certified when an equivalent is offered | EN 10204 3.1 |
Equivalents are the closest match by minimum strength, not identical grades β confirm chemistry, impact, thickness limits and testing on the mill test certificate (EN 10204 3.1).
Reviewed 26 Oct 2026