Choose a country to see its standard's plate, sheet and coil grades β and the closest match in the other seven systems.
European Committee for Standardization (CEN) Β· EN
β 250 MPa structural
S235JR / S275JR
Same class: ASTM A36 Β· IS E250 Β· AS/NZS 250 Β· GOST C245/C255 Β· GB/T Q235B Β· KS SS275 Β· JIS SS400
β 350 MPa structural
S355JR
Same class: ASTM A572 Gr 50 Β· IS E350 Β· AS/NZS 350 Β· GOST C345/09G2S Β· GB/T Q355B Β· KS SM355 Β· JIS SM490/SM490Y
Pressure vessel (β A516 Gr 70)
P355GH
Same class: ASTM A516 Gr 70 Β· IS R260 Β· GB/T Q345R Β· JIS SGV480
| Standard | Grades |
|---|---|
| Mild structural | |
| EN 10025-2 | S235, S275JR / J0 / J2 |
| High-strength / HSLA | |
| EN 10025-2 | S355JR / J0 / J2 / K2 |
| EN 10025-3 | S275 β S460N / NL β normalized |
| EN 10025-4 | S275 β S500M / ML β thermomechanical |
| EN 10025-6 | S460Q β S960QAlso QL / QL1 β quenched & tempered |
| Pressure vessel & boiler | |
| EN 10028-2 | P235GH, P265GH, P295GH, P355GH, 16Mo3, 13CrMo4-5 |
| EN 10028-3 | P275NH/NL1/NL2, P355N/NH/NL1/NL2 |
| Standard | Grades |
|---|---|
| Hot-rolled sheet & coil | |
| EN 10111 | DD11, DD12, DD13, DD14 |
| EN 10149-2 | S315MC β S700MC |
| Cold-rolled sheet & coil | |
| EN 10130 | DC01, DC03, DC04, DC05, DC06, DC07 |
| Hot-dip coated (zinc / Al-Zn) | |
| EN 10346 | DX51D β DX57D; S220GD β S550GD+Z / +AZ |
Ship plate uses the same IACS grades in every system: A, B, D, E and AH / DH / EH / FH 32 Β· 36 Β· 40 β certified by ABS, LR, DNV, BV, CCS, KR, NK or RS.
| Application | Specify | Note |
|---|---|---|
| Structural plate | ASTM A36 / A572 Gr 50 β or EN S275JR / S355JR | Most Saudi project specifications call ASTM or EN |
| Pressure-vessel plate | ASTM A516 Gr 70 | EN alternative: P355GH |
| Equivalent stock (GB/T, JIS, KS, IS) | Offer only as an approved equivalent | Dual-certified mill test certificate required |
| Item | What to state | Example |
|---|---|---|
| Standard & edition | Full designation with year | EN 10025-2:2019 |
| Grade | Strength grade | S355 |
| Sub-grade | Impact class / test temperature | J2 (27 J at β20 Β°C) |
| Size | Thickness Γ width Γ length | 20 Γ 2000 Γ 6000 mm |
| Certificate | Inspection document β dual-certified when an equivalent is offered | EN 10204 3.1 |
Equivalents are the closest match by minimum strength, not identical grades β confirm chemistry, impact, thickness limits and testing on the mill test certificate (EN 10204 3.1).
Reviewed 26 Oct 2026